What are the causes of dielectric withstand failure in vacuum circuit breakers?

Felix Spark
Felix Spark
Field: Failure and maintenance
China

Causes of Dielectric Withstand Failure in Vacuum Circuit Breakers:

  • Surface contamination: The product must be thoroughly cleaned before dielectric withstand testing to remove any dirt or contaminants.

Dielectric withstand tests for circuit breakers include both power-frequency withstand voltage and lightning impulse withstand voltage. These tests must be performed separately for phase-to-phase and pole-to-pole (across the vacuum interrupter) configurations.

Circuit Breaker Test Data.jpg

Circuit breakers are recommended to be tested for insulation while installed in switchgear cabinets. If tested separately, the contact parts must be insulated and shielded, typically using heat-shrink tubing or insulating sleeves. For fixed-type circuit breakers, testing is generally conducted by directly bolting the test leads to the pole column terminals.

For solid-insulated pole columns with vacuum interrupters, the vacuum interrupter itself does not require sheds (skirts) to increase creepage distance. The vacuum interrupter is encapsulated within epoxy resin using silicone rubber, so the outer surface of the interrupter does not bear voltage. Instead, flashover occurs along the outer surface of the solid-insulated pole column. Therefore, the creepage distance between the upper and lower terminals of the solid-insulated pole column must meet requirements. For a pole-to-pole spacing of 210 mm, after deducting the contact arm diameter of 50 mm, the creepage distance cannot exceed 240 mm if no sheds are present.

Circuit breaker.jpg

Since the contact arm and the pole column terminal cannot be fully sealed, the sheds in this section are critically important. For 40.5 kV applications, with a pole-to-pole spacing of 325 mm, even adding sheds cannot satisfy the required creepage distance, making surface flashover highly likely. Therefore, it is generally necessary to use compressed silicone rubber to form a sealed solid insulation at the joint between the contact arm and the pole column, completely preventing surface tracking along the pole column end face. After this treatment, the creepage distance between the upper and lower poles via the contact arm can meet requirements, avoiding discharge.

If the external insulation clearance and creepage distance of the solid-insulated pole column are sufficiently large, discharge typically will not occur. Dielectric strength reduction is usually caused by loss of vacuum in the interrupter or complete failure of the pole assembly. Cracks or housing defects resulting from improper design or manufacturing, early material aging due to processing issues, or vibration-induced flashover/breakdown can also lead to equipment damage.

For insulation-cylinder-type pole columns, both the inner and outer walls of the insulating cylinder must be considered for creepage distance. Therefore, products with a pole spacing of 205 mm are generally not available. Additionally, the vacuum interrupter itself must also provide sufficient creepage distance to prevent flashover between the upper and lower poles.

Circuit breaker Diagram.jpg

Moreover, material hygroscopicity can also cause insulation test failure. Although epoxy resin has certain water resistance, prolonged exposure to humid or wet environments allows water molecules to gradually penetrate into the resin, leading to hydrolysis that breaks chemical bonds and degrades performance—such as reduced adhesion and mechanical strength.

Circuit Breaker Test Data..jpg

Test Item Unit Test Method Index Value
Color / Visual Inspection As per specified color palette
Appearance / Visual Inspection Within limit
Density g/cm³ GB1033 1.7-1.85
Water Absorption % JB3961 ≤0.15
Shrinkage % JB3961 0.1-0.2
Impact Strength JK/m² GB1043 ≥25
Bending Strength Mpa JB3961 ≥100
Insulation Resistance Normal State Ω GB10064 ≥1.0×10¹³
After Immersion for 24h ≥1.0×10¹²
Electrical Strength
GB1408 ≥12
Arc Resistance S GB1411 180+
Comparative Tracking Index / GB4207 ≥600
Flammability / GB11020 FV0

Water is a good conductor of electricity. After absorbing moisture, the dielectric constant of epoxy resin increases and its insulation resistance decreases, which may lead to electrical leakage, breakdown, and other failures in electrical equipment. Moisture-absorbed epoxy resin in circuit breaker pole columns can trigger partial discharge, thereby shortening equipment service life.

Under high electric fields, moisture accelerates the growth of electrical trees, further degrading insulation performance. This is a common cause of epoxy resin insulation failure in power equipment.

Moisture absorption also promotes reactions between epoxy resin and other environmental factors (such as oxygen, acidic or alkaline substances), accelerating material aging, which manifests as yellowing and embrittlement.

For high-current solid-insulated pole columns, heat sinks are typically installed on the upper part. These heat sinks are usually made of aluminum and coated with epoxy fluidized insulation on the outer surface. Due to the thin walls of the heat sink fins, the electric field intensity remains high at the top—even though rounded edges are provided—making discharge likely.

Generally, discharge may occur between the heat sink and the metal shutter. In such cases, attention must be paid to the electrical clearance between them. The shutter should avoid sharp edges; instead, bent flat surfaces or similar designs can be used to improve the electric field distribution.

Give a tip and encourage the author!
Recommended
How to Inspect 10kV Vacuum Circuit Breakers Properly
How to Inspect 10kV Vacuum Circuit Breakers Properly
I. Inspection of Vacuum Circuit Breakers During Normal Operation1. Inspection in Closed (ON) Position The operating mechanism should be in the closed position; The main shaft roller should be disengaged from the oil damper; The opening spring should be in a charged (stretched) energy-stored state; The length of the moving contact rod of the vacuum interrupter protruding below the guide plate should be approximately 4–5 mm; The bellows inside the vacuum interrupter should be visible (this does no
Felix Spark
10/18/2025
Why Can't a 10kV VCB Trip Locally?
Why Can't a 10kV VCB Trip Locally?
The inability to manually operate the local mechanical trip of a 10kV vacuum circuit breaker is a relatively common fault type in power system maintenance work. Based on years of field experience, such issues typically stem from five core areas, each requiring troubleshooting based on specific symptoms.Operating mechanism jamming is the most common cause. The tripping process of a circuit breaker relies on mechanical energy released from spring energy storage; if rust, deformation, or foreign ob
Felix Spark
10/18/2025
How to Choose Vacuum Circuit Breakers Correctly?
How to Choose Vacuum Circuit Breakers Correctly?
01 PrefaceIn medium-voltage systems, circuit breakers are indispensable primary components. Vacuum circuit breakers dominate the domestic market. Therefore, correct electrical design is inseparable from the proper selection of vacuum circuit breakers. In this section, we will discuss how to correctly select vacuum circuit breakers and common misconceptions in their selection.02 Interrupting Capacity for Short-Circuit Current Need Not Be Excessively HighThe short-circuit interrupting capacity of
James
10/18/2025
Vacuum vs Air Circuit Breakers: Key Differences
Vacuum vs Air Circuit Breakers: Key Differences
Low-Voltage Air Circuit Breakers vs. Vacuum Circuit Breakers: Structure, Performance and ApplicationLow-voltage air circuit breakers, also known as universal or molded frame circuit breakers (MCCBs), are designed for AC voltages of 380/690V and DC voltages up to 1500V, with rated currents ranging from 400A to 6300A or even 7500A. These breakers use air as the arc-quenching medium. The arc is extinguished through arc elongation, splitting, and cooling by an arc chute (arc runner). Such breakers c
Garca
10/18/2025
Related Products
Send inquiry
Download
Get the IEE Business Application
Use the IEE-Business app to find equipment, obtain solutions, connect with experts, and participate in industry collaboration anytime, anywhere—fully supporting the development of your power projects and business.